Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000587 ohm-cm | 0.0000587 ohm-cm | |
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab.. |
|||
Electrical Resistivity | 0.0000587 ohm-cm | 0.0000587 ohm-cm | |
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |