Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, 1/4 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, 3/4 Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, Annealed 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, Extra Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, Extra Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Electrical Resistivity | 0.0000324 ohm-cm | 0.0000324 ohm-cm | Annealed |
Eagle Brass 770 Nickel Silver 18%, Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |