Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Electrical Resistivity | 0.00001187 ohm-cm | 0.00001187 ohm-cm | Annealed |
Eagle Brass 510 Phosphor Bronzes 5% A, Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |