Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000750 - 0.00000810 ohm-cm | 0.00000750 - 0.00000810 ohm-cm | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Electrical Resistivity | 0.00000750 - 0.00000810 ohm-cm | 0.00000750 - 0.00000810 ohm-cm | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Electrical Resistivity | 0.00000750 - 0.00000960 ohm-cm | 0.00000750 - 0.00000960 ohm-cm | 18-23% IACS Conductivity |
Materion Beryllium Copper Alloy 245C Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Electrical Resistivity | 0.00000750 - 0.00000960 ohm-cm | 0.00000750 - 0.00000960 ohm-cm | 18-23% IACS Conductivity |
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600) Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula.. |
|||
Electrical Resistivity | 0.00000750 ohm-cm | 0.00000750 ohm-cm | |
Indium Corp. Indalloy® 290 In-Ag Solder Alloy Indium with silver added to improve strength. Has the wettability and low-temperature malleability of indium. Particularly useful for cryogenic applications.Information provided by the manufacturer,.. |
|||
Electrical Resistivity | 0.00000750 ohm-cm | 0.00000750 ohm-cm | |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Electrical Resistivity | 0.00000750 ohm-cm | 0.00000750 ohm-cm | Forgings (23 % IACS) |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |