Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000520 ohm-cm | 0.00000520 ohm-cm | 33 % IACS |
CMW® ELKON 100M Pure Molybdenum Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The elec.. |