Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000340 ohm-cm | 0.00000340 ohm-cm | |
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
Electrical Resistivity | 0.00000340 ohm-cm | 0.00000340 ohm-cm | |
Hogen H20S, 26 Silver/74 Tungsten PM Metal Composite RWMA Class EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica.. |
|||
Electrical Resistivity | 0.00000340 - 0.00000380 ohm-cm | 0.00000340 - 0.00000380 ohm-cm | 45-50% IACS Conductivity |
Materion Beryllium Copper Alloy 10C Castings (UNS C82000) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul.. |
|||
Electrical Resistivity | <= 0.00000340 ohm-cm | <= 0.00000340 ohm-cm | 50% IACS conductivity (minimum) |
Materion Brush 60™ HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
Electrical Resistivity | 0.00000340 ohm-cm | 0.00000340 ohm-cm | |
Mi-Tech Metals CW68 68 Tungsten/32 Copper PM Metal Composite RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme.. |
|||
Electrical Resistivity | 0.00000340 ohm-cm | 0.00000340 ohm-cm | |
Mi-Tech Metals SW74 26 Silver/74 Tungsten PM Metal Composite RWMA Class EDMMi-Tech Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica.. |
|||
Electrical Resistivity | <= 0.00000340 ohm-cm | <= 0.00000340 ohm-cm | 50% IACS conductivity (minimum) |
Materion Brush 60™ 3/4 HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
Electrical Resistivity | 0.00000340 ohm-cm | 0.00000340 ohm-cm | Temper T651 |
Constellium DOKIMA® Rolled Plate Aluminum DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct.. |
|||
Electrical Resistivity | 0.00000340 ohm-cm | 0.00000340 ohm-cm | 51 % IACS |
CMW® ELKONITE 35SB tungsten, silver ELKONITE® 35SB is the most popular material made by the press sinter process with a small addition of nickel used to activate the sintering. Because of fewer steps in manufacture this material is m.. |