Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915â„¢ Annealed Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915â„¢ Annealed Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915™ AT Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915™ AT Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915™ Heat Treated Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | (55% IACS Conductivity) |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Electrical Resistivity | 0.00000310 ohm-cm | 0.00000310 ohm-cm | 55 % IACS |
CMW® ELKONITE 40SB tungsten, silver Information provided by CMW Inc. |