Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000169 ohm-cm | 0.00000169 ohm-cm | (102% IACS) |
CMW® D581F Silver Graphite Contact Material For electrical contacts; reduced sticking, low friction.Information provided by CMW Inc. |