Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc Resistance to Ignition (HVAR) | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746A |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |