Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.70 mm |
60 - 120 arcs @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
PLC 1 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 2.50 mm |
60 - 120 arcs @Thickness 0.0984 in |
PLC 1 |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 2.50 mm |
60 - 120 arcs @Thickness 0.0984 in |
PLC 1 |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 0.710 mm |
60 - 120 arcs @Thickness 0.0280 in |
|
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
|
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
High Amp Arc Ignition, HAI | 60 - 119 arcs @Thickness 1.50 mm |
60 - 119 arcs @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |