Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 0.550 mm |
15 - 30 arcs @Thickness 0.0217 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
BK |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |