Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.800 mm |
7.0 - 15 sec @Thickness 0.0315 in |
UL 746 |
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.851 mm |
7.0 - 15 sec @Thickness 0.0335 in |
UL 746 |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.550 mm |
7.0 - 15 sec @Thickness >=0.0217 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.800 mm |
7.0 - 15 sec @Thickness >=0.0315 in |
|
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
UL 746A |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |