Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.800 mm |
7.0 - 15 sec @Thickness 0.0315 in |
UL 746 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.800 mm |
7.0 - 15 sec @Thickness >=0.0315 in |
|
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FG PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 3.00 mm |
7.0 - 15 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 3.00 mm |
7.0 - 15 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |