Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 2.50 mm |
15 - 30 sec @Thickness 0.0984 in |
PLC 3 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.50 mm |
15 - 30 sec @Thickness >=0.0984 in |
|
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.50 mm |
15 - 30 sec @Thickness >=0.0984 in |
|
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=6.00 mm |
15 - 30 sec @Thickness >=0.236 in |
|
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2156FL PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.00 mm |
15 - 30 sec @Thickness >=0.0787 in |
|
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.00 mm |
15 - 30 sec @Thickness >=0.0787 in |
|
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 0.750 mm |
15 - 30 sec @Thickness 0.0295 in |
PLC 3 |
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |