Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |