Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.851 mm |
7.0 - 15 sec @Thickness 0.0335 in |
UL 746 |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.851 mm |
7.0 - 15 sec @Thickness 0.0335 in |
UL 746 |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=2.50 mm |
7.0 - 15 sec @Thickness >=0.0984 in |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FG PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
All colors |
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
UL 746A |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.710 mm |
7.0 - 15 sec @Thickness 0.0280 in |
UL 746B |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 3.00 mm |
7.0 - 15 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |