Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 14 - 29 sec @Thickness 3.00 mm |
14 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Hot Wire Ignition, HWI | 14 - 29 sec @Thickness 3.00 mm |
14 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |