Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 382 - 404 °C | 720 - 760 °F | Molding |
PolyOne Edgetek® PK-15CF-15GB/000 Polyetheretherketone (PEEK), Glass Bead, Carbon Fiber Reinforced
(discontin Description/Features:Carbon Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |