Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Temperature | 371 - 399 °C | 700 - 750 °F | Stock |
PolyOne Lubri-Tech™ PK-000/15T Polyetheretherketone - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 371 - 399 °C | 700 - 750 °F | Molding |
PolyOne Edgetek® ES-40CF/000 Polyethersulfone - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
Clariant Renol PEEKSP003 Polyetheretherketone, Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 340 - 399 °C | 644 - 750 °F | Average value: 363 °C Grade Count:16 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Melt Temperature | 338 - 399 °C | 640 - 750 °F | |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |