Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne OnForce™ LFT SF-40LGF/001 Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | Injection Molding |
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Melt Temperature | 310 - 340 °C | 590 - 644 °F | |
LATI Laramid CE/60 PPA, 60% Mineral Reinforced Semi-aromatic polyamide (PPA) based compound. Mineral filler. High dimensional stability. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Melt Temperature | 310 - 340 °C | 590 - 644 °F | |
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af.. |
|||
Melt Temperature | 310 - 340 °C | 590 - 644 °F | |
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
Covestro Apec® 1703 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content |
|||
Melt Temperature | 330 - 340 °C | 626 - 644 °F | |
Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
Melt Temperature | 330 - 340 °C | 626 - 644 °F | |
Covestro Apec® DP1-9389/5 Polycarbonate Developmental producteasy flowingeasy to demoldsoftening temperature (VST/B 120)=218 °CPreprocessingMax. Water content |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |