Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 280 - 310 °C | 536 - 590 °F | |
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove.. |
|||
Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Melt Temperature | 243 - 310 °C | 469 - 590 °F | Average value: 284 °C Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Melt Temperature | 250 - 310 °C | 482 - 590 °F | |
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin
(discontinued **) Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng.. |
|||
Melt Temperature | 280 - 310 °C | 536 - 590 °F | |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Melt Temperature | 275 - 310 °C | 527 - 590 °F | Start Point: 285°C |
Kingfa PA66-G50 50% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Melt Temperature | 295 - 310 °C | 563 - 590 °F | Injection Molding |
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 295 - 310 °C | 563 - 590 °F | |
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Melt Temperature | 300 - 310 °C | 572 - 590 °F | |
Samyang Trirex® 3022L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 288 - 310 °C | 550 - 590 °F | |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 280 - 310 °C | 536 - 590 °F | |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Melt Temperature | 280 - 310 °C | 536 - 590 °F | Injection Molding/Extrusion |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |