Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 255 - 285 °C | 491 - 545 °F | |
PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 232 - 285 °C | 450 - 545 °F | Average value: 263 °C Grade Count:8 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Melt Temperature | 245 - 285 °C | 473 - 545 °F | Injection Molding |
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p.. |
|||
Melt Temperature | 255 - 285 °C | 491 - 545 °F | Injection Molding |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Melt Temperature | 265 - 285 °C | 509 - 545 °F | |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Melt Temperature | 255 - 285 °C | 491 - 545 °F | Start Point: 265°C |
Kingfa CPA-6 Toughened PA6 Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Temperature | 280 - 285 °C | 536 - 545 °F | |
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |
|||
Melt Temperature | 245 - 285 °C | 473 - 545 °F | |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Temperature | 270 - 285 °C | 518 - 545 °F | |
Eurostar Starflam AFR560B1 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B1 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 285 °C | 518 - 545 °F | |
Eurostar Starflam AFR560B5 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B5 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 185 - 285 °C | 365 - 545 °F | Extrusion Coating |
DuPont™ Surlyn® 6320 Magnesium Ionomer Surlyn® 6320 is a magnesium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 6320 thermoplastic r.. |
|||
Melt Temperature | 240 - 285 °C | 464 - 545 °F | |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |