Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1511 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3601 General Purpose Crystal Polystyrene
(discontinued **) Easy flow for high productivity, excellent post molding scuff resistanceApplications: Medical, LabwareExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phys.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5751 High Impact Polystyrene
(discontinued **) High flow, Good impact, USP Class VIApplications: Single service impact, Medical, Housewares, CompoundingProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwi.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 602 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Melt Temperature | 221 - 274 °C | 430 - 525 °F | Average value: 249 °C Grade Count:5 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Melt Temperature | 221 - 274 °C | 430 - 525 °F | Average value: 249 °C Grade Count:13 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | Injection Molding |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3100 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 4210 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5420 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5620 High Impact Polystyrene
(discontinued **) High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 6100 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 202 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Fast cyclingApplications: XPS food packaging, Foam insulation, CD boxes, medical and food disposables, Sheet and profile extrusionProperties were determined on injection m.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 202W Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulationProperties were determined on injection molded specimens at 23° and 50% RH unless otherwise specified.Information provi.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 204L Crystal Polystyrene General Purpose Grade
(discontinued **) Fast cycling, Good heat resistance, Good balance of properties and flow characteristics, Extrusion and Injection Molding Applications: General purpose injection molded itemsProperties were determin.. |