Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 232 - 257 °C | 450 - 495 °F | |
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color .. |
|||
Melt Temperature | 247 - 257 °C | 477 - 495 °F | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |