Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 191 - 229 °C | 376 - 444 °F | Injection |
Samsung Cheil Industries Starex® SD-0150 ABS, Unreinforced
(discontinued **) Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: General Purpose: Good Impact Strength, Chemical Resistance, ProcessabilityApplications: Household Appliances, Auto Interior Trim and P.. |