Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Melt Temperature | 193 - 221 °C | 379 - 430 °F | |
PolyOne Edgetek® PE-30GF/000 Polyethylene, High Density (HDPE) Information provided by PolyOne |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | |
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4480 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4480 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 210 - 221 °C | 410 - 430 °F | Molding |
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Melt Temperature | 204 - 221 °C | 400 - 430 °F | |
Ecomass® 4703BI74 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Melt Temperature | 191 - 221 °C | 375 - 430 °F | |
Clariant Remafin PP1100NAT Polypropylene Impact Modified Copolymer Data provided by Clariant Masterbatches |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | |
M. Holland Company LL106 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | |
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based
(discontinued **) Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | |
Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2101-85A offers good low temperature properties, fast cycle time, and good hydrolytic stability. Applications include: seals, gaskets, animal tags, molding applications, ho.. |