Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne LubriOne™ ATH-000/18T 2S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 182 - 216 °C | 360 - 421 °F | |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Melt Temperature | 182 - 216 °C | 360 - 421 °F | |
PolyOne Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where excepti.. |
|||
Melt Temperature | 213 - 216 °C | 415 - 421 °F | |
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
Melt Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 188 - 216 °C | 370 - 421 °F | Stock |
PolyOne Lubri-Tech™ ATH-000/02T Homopolymer - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 193 - 216 °C | 379 - 421 °F | Stock |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 188 - 216 °C | 370 - 421 °F | Stock |
PolyOne Lubri-Tech™ ATH-000/20T Homopolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 199 - 216 °C | 390 - 421 °F | Typical Extrusion |
LyondellBasell Alathon® L5045 High Density Polyethylene ApplicationsALATHON L 5045 is a medium molecular weight high density polymer for use in blown film extrusion applications. Typical applications include millinery bags, coextrusions and plastic nett.. |
|||
Melt Temperature | 199 - 216 °C | 390 - 421 °F | Typical Extrusion |
LyondellBasell Alathon® L5845 High Density Polyethylene ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg.. |
|||
Melt Temperature | 199 - 216 °C | 390 - 421 °F | |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |
|||
Melt Temperature | 199 - 216 °C | 390 - 421 °F | Molding |
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Melt Temperature | 199 - 216 °C | 390 - 421 °F | Extrusion |
Lubrizol Estane® 2355-55DE Thermoplastic Polyurethane Type: Pellethane® 2355-55DE is a thermoplastic polyurethane elastomer.Information Provided by The Lubrizol Corporation |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Melt Temperature | 143 - 216 °C | 289 - 421 °F | Processing |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Melt Temperature | 199 - 216 °C | 390 - 421 °F | Molding |
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod.. |
|||
Melt Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |