Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 188 - 210 °C | 370 - 410 °F | |
PolyOne LubriOne™ AT-000/10T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 170 - 210 °C | 338 - 410 °F | |
PolyOne OnFlex™ U 5355A-S0014 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of.. |
|||
Melt Temperature | 185 - 210 °C | 365 - 410 °F | |
Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
Melt Temperature | 199 - 210 °C | 390 - 410 °F | |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 160 - 210 °C | 320 - 410 °F | Extrusion |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-1267A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-1273A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-1654A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-1934A Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Flexible Cord Jacketing; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581Forms: P.. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-2570F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-2696A Thermoplastic Elastomer Uses: Cell Phones; Consumer Applications; General Purpose; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes.. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-3954-80 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-6065 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-83-F912-E-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-88-N809K Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
Teknor Apex Telcar® TL-2270A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Temperature | 182 - 210 °C | 360 - 410 °F | |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |