Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8600-60 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8915-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8925-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8950-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8960-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8980-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 8999-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9600-60 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9915-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9925-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9940-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9950-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9960-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 154 - 166 °C | 310 - 330 °F | |
Sylvin Technologies 9980-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC1390AA Low Density Polyethylene WESTLAKE low-density polyethylene EC1390 is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density po.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC1924AA Low Density Polyethylene WESTLAKE low-density polyethylene EC1924 is a resin that is widely used in the boardstock coating industry. This material has an excellent combination of low neck-in, ease of processing, good chill-.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC4042AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4042 is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combi.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC4056AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC800AA Low Density Polyethylene WESTLAKE low-density polyethylene EC800 is a general-purpose low-density formulation used for extrusion coating applications.Application/UsesGeneral extrusion coatingFDA: This material complies with.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC811AA Low Density Polyethylene WESTLAKE low-density polyethylene EC811 is used for extrusion coating applications. It exhibits good adhesion, low coat weight, and fast heat seals.Application/UsesCoatings for paper/paperboardFDA: .. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC812AA Low Density Polyethylene WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC850AA Low Density Polyethylene WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides goo.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM1550AA Low Density Polyethylene WESTLAKE low-density polyethylene EM1550 is a low-density formulation used for injection molding applications.Application/UsesFlexible medicalLidsMedicalFDA: This material complies with FDA regulati.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM182AA Low Density Polyethylene WESTLAKE low-density polyethylene EM182 is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM184AA Low Density Polyethylene WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM1870AA Low Density Polyethylene WESTLAKE low-density polyethylene EM1870 is used for injection molding applications. It has excellent stress crack resistance for lids.Application/UsesFlexible medicalLidsMedicalFDA: This material c.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM800AA Low Density Polyethylene WESTLAKE low-density polyethylene EM800 is a general-purpose low-density formulation used for injection molding applications that require good stress-crack resistance.Application/UsesCosmetics/perso.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM808AA Low Density Polyethylene WESTLAKE low-density polyethylene EM808 is a general-purpose low-density formulation used for injection molding applications and general purpose extrusion.Application/UsesFood packagingMedicalFDA: T.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM811AA Low Density Polyethylene WESTLAKE low-density polyethylene EM811 is a low-density polyethylene used for injection molding. It is characterized by high flow and low stiffness.Application/UsesFlexible medicalMedicalFDA: This .. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM812AA Low Density Polyethylene WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi.. |