Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 1110 - 1280 °C | 2030 - 2340 °F | |
Wieland Duo Pal 6 PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |