Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 1060 - 1180 °C | 1940 - 2160 °F | |
Wieland Porta AB 76 Casting Alloy Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, ceramic veneering, acrylic veneeringDental |
|||
Melt Temperature | 1080 - 1180 °C | 1980 - 2160 °F | |
Wieland Porta PressOver PFM Alloy High gold alloy for veneering with IMAGINE® h.e. press ceramicApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, acrylic veneeringDental |