Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 90.0 - 100 °C | 194 - 212 °F | Injection molding |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free
(discontinued **) Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage
(discontinued **)& Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 14600 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, low specific gravity.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a part of Hexion in 2005.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak .. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Melt Temperature | 70.0 - 100 °C | 158 - 212 °F | Injection molding |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
|||
Melt Temperature | 90.0 - 100 °C | 194 - 212 °F | Injection molding |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed
&n Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte.. |