Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
PolyOne Bergamid™ A700 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Melt Temperature | 270 °C | 518 °F | Injection Molding; ISO 294 |
Lanxess Pocan® T 7391 POS151 000000 PBT + PET, 45% Glass Fiber
(discontinued **) PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Melt Temperature | 270 - 327 °C | 518 - 620 °F | Average value: 303 °C Grade Count:45 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Melt Temperature | <= 270 °C | <= 518 °F | |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Melt Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Melt Temperature | 270 °C | 518 °F | for test specimens; ISO 294 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | ISO 294 |
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | ISO 294 |
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab.. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide A28K PA66, Heat Stabilized, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide ACF6 PA66, 30% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF6 is a 30% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 285 °C | 518 - 545 °F | |
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
E-Polymers TEKANATE® G7038 High Easy Molding Polycarbonate Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows .. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection-molding/Extrusion |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection-molding/Extrusion |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Melt Temperature | 270 °C | 518 °F | for shrinkage test |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection-molding/Extrusion |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection-molding/Extrusion |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
Melt Temperature | 270 - 310 °C | 518 - 590 °F | Average value: 288 °C Grade Count:23 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Melt Temperature | 270 °C | 518 °F | for shrinkage test, Optimal |
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab.. |
|||
Melt Temperature | 270 °C | 518 °F | Injection Molding; ISO 294 |
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber
(discontinued **) PBT+ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish |