Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 268 - 293 °C | 515 - 560 °F | |
LTL Color Compounds ColorFast® NY2115 Nylon 66 Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc. |