Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 235 - 260 °C | 455 - 500 °F | Start Point: 240°C |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Melt Temperature | <= 235 °C | <= 455 °F | CoExtrusion with EVA Processing |
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Temperature | 235 - 310 °C | 455 - 590 °F | Extrusion Coating |
DuPont™ Elvaloy® AC 2618 Ethylene Methyl Acrylate Elvaloy® AC 2618 is a copolymer of ethylene and ethyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC.. |
|||
Melt Temperature | 235 °C | 455 °F | |
Polyplastic Armlen® PP MF 20-3-901 Polypropylene, 20% Mineral Filled Heat stabilized, low emission, black colorInformation provided by PolyPlastic Group. |