Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 170 - 210 °C | 338 - 410 °F | |
PolyOne OnFlex™ U 5355A-S0014 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2807 HDPE Injection Molding Resin Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Industrial and lubricant pails.Data provided by .. |
|||
Melt Temperature | 170 - 185 °C | 338 - 365 °F | |
SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Melt Temperature | 170 - 220 °C | 338 - 428 °F | |
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin
(discontinued **) LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,.. |
|||
Melt Temperature | 170 - 220 °C | 338 - 428 °F | |
Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin
(discontinued **) LI5011 is a pelleted high flow linear low density polyethylene. The higher melting point of the resin allows for higher end-use temperatures.Applications: House-wares, toys, lids, containers.Advan.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Melt Temperature | 170 - 260 °C | 338 - 500 °F | |
NOVA Chemicals Sclair® 2717 HDPE Injection Molding Resin
(discontinued **) Features: Super high flow, good balance of toughness and stiffness, low odor, permits container weight reduction.Applications: Thin walled food containers.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2607 HDPE Injection Molding Resin Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2607-UV14 HDPE Injection Molding Resin Excellent stiffness, Good impact resistance, Low warpageApplications: Roll-out cartsAdditives: Elevated levels of ultraviolet stabilizer packages, Elevated levels of antioxidantsInformation provided.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8406 BK, 8406 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 222 °C Grade Count:70 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Melt Temperature | 170 - 200 °C | 338 - 392 °F | |
Borealis BS2581 High Density Polyethylene for Blow Molding BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol.. |
|||
Melt Temperature | 170 - 200 °C | 338 - 392 °F | |
Borealis FA3227 Low Density Polyethylene FA3227 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Heat and U/V stabilized. This grade is suitable for building construction film and meets the requirements for heat, al.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 220 °C | 338 - 428 °F | Average value: 200 °C Grade Count:14 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Melt Temperature | 170 - 260 °C | 338 - 500 °F | |
NOVA Chemicals Sclair® 2715 HDPE Injection Molding Resin
(discontinued **) Features: Excellent low temperature impact strength, good balance of toughness and stiffness, low odor.Applications: Thin walled food containers and lids, frozen and refrigerated containers.Data pro.. |