Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 130 - 280 °C
266 - 536 °F
Average value: 193 °C Grade Count:55
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Melt Temperature 130 °C
266 °F
Iran Petrochemical (PCC) HB0035 High Density Polyethylene
HB0035 is a high molecular weight high density polyethylene blow molding grade combining blow molding extrusion behavior and superior mechanical properties. Blow molded items made from HB 0035 exhi..
Melt Temperature 130 °C
266 °F
Iran Petrochemical (PCC) 5030UA High Density Polyethylene
HD-5030UA is a high-density polyethylene copolymer grade with a narrow molecular weight distribution, specially developed for injection molding application requiring very high environmental stress c..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable
LE4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications LE4201R is intended for insulation of XLPE power cables with rated voltages up..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis LE4244R Polyethylene Insulation Compound, Crosslinkable
LE4244R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. This product is only available in certain periods. Applications: LE4244R is intended for in..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis Superclean™ LE4201EHV Polyethylene Insulation Compound, Crosslinkable
Superclean™ LE4201EHV is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Superclean™ LE4201EHV is intended for insulation of XLPE extr..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis Superclean™ LE4244S Polyethylene Insulation Compound, Crosslinkable
Superclean™ LE4244S is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Superclean™ LE4244S is intended for insulation of XLPE High Vol..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis SuperCOPO™ LE4205R Polyethylene Insulation Compound, Crosslinkable
SuperCOPO™ LE4205R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LE4205R is intended for insulation of XLPE power cabl..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis SuperCOPO™ LH4201R Polyethylene Insulation Compound, Crosslinkable
SuperCOPO™ LH4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LH4201R is intended for insulation of XLPE power cabl..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis Supercure™ LE8201R Polyethylene Insulation Compound, Crosslinkable
Supercure™ LE8201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Supercure™ LE8201R is recommended for use with Supercure™ LE8280 as shielding..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis Superclean™ LE4244EHV Polyethylene Insulation Compound, Crosslinkable
Superclean™ LE4244EHV is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Superclean™ LE4244EHV is intended for insulation of XLPE extr..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis Supercure™ LS4201R Polyethylene Insulation Compound, Crosslinkable
Supercure™ LS4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Supercure™ LS4201R is intended for insulation of XLPE power cabl..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis Supercure™ LS4201S Polyethylene Insulation Compound, Crosslinkable
Supercure™ LS4201S is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Supercure™ LS4201S is intended for insulation of XLPE High Volta..
Melt Temperature 130 - 140 °C
266 - 284 °F
Borealis Supersmooth™ LE8280 Polyethylene Insulation Compound, Crosslinkable
Supersmooth™ LE8280 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE8280 is intended for semiconduct..