Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 1080 - 1180 °C | 1980 - 2160 °F | |
Wieland Porta PressOver PFM Alloy High gold alloy for veneering with IMAGINE® h.e. press ceramicApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, acrylic veneeringDental |
|||
Melt Temperature | 1080 - 1200 °C | 1980 - 2190 °F | |
Wieland Simidur S 1S PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |