Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 70.0 - 343 °C | 158 - 650 °F | Average value: 307 °C Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Melt Temperature | 70.0 - 325 °C | 158 - 617 °F | Average value: 282 °C Grade Count:14 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Melt Temperature | 70.0 - 315 °C | 158 - 599 °F | Average value: 290 °C Grade Count:33 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 70.0 - 100 °C | 158 - 212 °F | Injection molding |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
|||
Melt Temperature | 70.0 - 260 °C | 158 - 500 °F | Average value: 229 °C Grade Count:43 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |