Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 360 - 404 °C | 680 - 759 °F | Average value: 374 °C Grade Count:6 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Melt Temperature | 382 - 404 °C | 720 - 760 °F | Molding |
PolyOne Edgetek® PK-15CF-15GB/000 Polyetheretherketone (PEEK), Glass Bead, Carbon Fiber Reinforced
(discontin Description/Features:Carbon Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 382 - 404 °C | 720 - 759 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Melt Temperature | 382 - 404 °C | 720 - 759 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Melt Temperature | 382 - 404 °C | 720 - 759 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Melt Temperature | 382 - 404 °C | 720 - 759 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Melt Temperature | 382 - 404 °C | 720 - 759 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable.. |
|||
Melt Temperature | 382 - 404 °C | 720 - 759 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Melt Temperature | 382 - 404 °C | 720 - 759 °F | |
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
(discontinued **) Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still.. |