Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-4 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-100NL Nucleated, Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-1010 Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond) Information provided by Ravago |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
LTL Color Compounds ColorFast® PC200 Polycarbonate 20 melt superior processing, fast cyclingAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package .. |
|||
Melt Temperature | 277 - 293 °C | 530 - 560 °F | |
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman EcoLon® MRGF1518-BK Mineral/Glass Fiber Reinforced Nylon 66, Lubricated, Heat Stabilized, PCR Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
Clariant Renol 66G15BL-195 Blue Nylon 66, 15% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
Clariant Renol 6601M Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 216 - 293 °C | 420 - 560 °F | Average value: 247 °C Grade Count:9 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 260 - 293 °C | 500 - 559 °F | |
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued 12 wt% Methacrylic Acid.Nucrel® 1207 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des.. |