Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
PolyOne Edgetek® XT XT-115GF-AX00 PC+PBT with Glass Fiber Reinforcement
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
PolyOne Edgetek® XT XT-115GF-AX01-HF PC+PBT with Glass Fiber Reinforcement
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Melt Temperature | 170 - 282 °C | 338 - 540 °F | Average value: 219 °C Grade Count:44 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 266 - 282 °C | 510 - 540 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 271 - 282 °C | 520 - 540 °F | |
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 260 - 282 °C | 500 - 540 °F | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Melt Temperature | 263 - 282 °C | 505 - 540 °F | Processing Temperature |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Melt Temperature | 263 - 282 °C | 505 - 540 °F | Processing Temperature |
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Melt Temperature | 249 - 282 °C | 480 - 540 °F | |
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Clariant Renol BR7140 Polycarbonate/ABS Alloy Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Melt Temperature | 246 - 282 °C | 475 - 540 °F | |
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 249 - 282 °C | 480 - 540 °F | |
Styron EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated.. |