Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
LG Chemical LUPOY ER5151RFA PC/ABS Mineral Filler, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High strength, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 14807-96-6Information p.. |
|||
Melt Temperature | 255 - 275 °C | 491 - 527 °F | |
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d.. |
|||
Melt Temperature | 255 - 275 °C | 491 - 527 °F | Start Point: 260°C |
Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 210 - 275 °C | 410 - 527 °F | |
Borealis MG7547B Polyethylene MG7547B is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Melt Temperature | 210 - 275 °C | 410 - 527 °F | |
Borealis MG9641S Polyethylene MG9641S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Melt Temperature | 210 - 275 °C | 410 - 527 °F | |
Borealis MG9647B Polyethylene MG9647B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 260 - 275 °C | 500 - 527 °F | |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Starflam PX05004 PA66, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding/Extrusion |
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding/Extrusion |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® B 4406 G2 10% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 10% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding/Extrusion |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection Molding |
LG Chemical LUPOY NS5000C PC/ABS, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding/Extrusion |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Melt Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |