Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 250 - 265 °C | 482 - 509 °F | |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Melt Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUMID HI5001AS PA6/PO, High Barrier Property, CaCl2 Resistance, High Impact Feature: Injection Molding, PA6/PO, High Barrier Property, CaCl2 Resistance, High ImpactApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1, 9002-88-4 and 105-60-2Information pro.. |
|||
Melt Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided .. |
|||
Melt Temperature | 255 - 265 °C | 491 - 509 °F | Injection Molding |
LG Chemical Lupox® SG5150 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good SurfaceApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5100 PC/ABS+GF10% Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by.. |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Melt Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Melt Temperature | 255 - 265 °C | 491 - 509 °F | |
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Melt Temperature | 255 - 265 °C | 491 - 509 °F | |
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo. |
|||
Melt Temperature | 255 - 265 °C | 491 - 509 °F | |
Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessInformation provided by Toyobo. |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | |
CP-Polymer-Technik Wellamid® 6000 HWCP Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | |
CP-Polymer-Technik Wellamid® 6000 HWUVCP Nylon 6, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 255 - 265 °C | 491 - 509 °F | |
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 250 - 265 °C | 482 - 509 °F | |
Ecomass® 705BI79 BaSO4 Filled ABS Nontoxic alternative to traditional materials, radiation shielding applications.Moderate Specific GravityBaSO4 Powder Filled ABSInformation provided by Technical Polymers |
|||
Melt Temperature | 188 - 265 °C | 370 - 509 °F | Average value: 220 °C Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |