Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPC BGK601213 CR Polypropylene Copolymer, Multifiller Information provided by Polykemi AB |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 240°C |
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Melt Temperature | 210 - 260 °C | 410 - 500 °F | Injection |
Inno-Comp INNOPOL® CS 2-3110 TO BU 10% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-3110 TO BU is a 10% talc-filled, black colored and UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3110 TO BU is developed for producing injection mol.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Sax Polymers SAXLAC 120U Acrylonitrile Butadiene Styrene Saxalac 120U is an UV protected easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Melt Temperature | 210 - 260 °C | 410 - 500 °F | |
Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications Bormed HF840MO is a polypropylene homopolymer intended for injection molding and is modified with an internal lubricant for products requiring a low surface friction (e.g. two-part syringes).Bormed .. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Borealis HE125MO Polypropylene HE125MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by good flow properties and high stiffness in and is specially suitable for high-speed injection mo.. |
|||
Melt Temperature | 252 - 260 °C | 485 - 500 °F | |
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
A. Schulman VOLOY™ 461 Glass Reinforced, Flame Retardant PBT Alloy Information provided by A. Schulman. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | |
Entec Hylox® 9020 PBT, 20% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide B28 PA6, Injection Molded Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Clariant Renol PA2SP0009HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Clariant Renol 6004G23 Nylon 6, 23% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
BLUESTAR PBT 6630 30% Glass Filled PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, E/E industry.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | Injection-molding/Extrusion |
BASF Ultramid® Seal-Fit PA6/66 (Conditioned) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |