Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 235 - 255 °C | 455 - 491 °F | Start Point: 250°C |
Kingfa UTPBT-HB Toughened PBT Features:High impactExcellent size stabilityEasy processingApplications:Injection moldingSwitch partsKeyboard keysE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2300R PBT+GF30% Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® HI2100M PBT+GF10% Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® LW5402A PBT+PC+GF40% Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3180S PBT+PET+MF18% Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3250A PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2156FM PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
Melt Temperature | 235 - 255 °C | 455 - 491 °F | EBM |
Eastman Tritan TX1801 Copolyester, Natural Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo.. |