Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 221 - 249 °C | 430 - 480 °F | |
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP 1141 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP 1227D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1473 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1564-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1580D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1627 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1671 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1695L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1791R4 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1838-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1878B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2207B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2239 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2253 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2295 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2327-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP 1097F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-1852A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2359A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2564B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2755 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-4123 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
Teknor Apex Monprene® MP-2890M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Temperature | 182 - 249 °C | 360 - 480 °F | Average value: 223 °C Grade Count:5 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |
|||
Melt Temperature | 191 - 249 °C | 375 - 480 °F | Average value: 224 °C Grade Count:7 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |