Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 149 - 232 °C | 300 - 450 °F | |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Melt Temperature | 210 - 232 °C | 410 - 450 °F | |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 199 - 232 °C | 390 - 450 °F | |
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 199 - 232 °C | 390 - 450 °F | |
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Melt Temperature | 200 - 232 °C | 392 - 450 °F | Injection |
Total PPH 3720WZ Polypropylene, Injection Molding Grade High flow reactor injection molding homopolymerHigh Flow - FINA 3720WZ has high flow characteristics that result in ease of filling thin wall parts.Nucleation - FINA 3720WZ is nucleated to provide f.. |
|||
Melt Temperature | 193 - 232 °C | 380 - 450 °F | Processing |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Melt Temperature | 193 - 232 °C | 380 - 450 °F | Processing |
ExxonMobil Santoprene® 241-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | Average value: 193 °C Grade Count:3 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |