Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 195 - 225 °C | 383 - 437 °F | |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
Melt Temperature | 200 - 225 °C | 392 - 437 °F | |
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Temperature | 200 - 225 °C | 392 - 437 °F | |
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Temperature | 200 - 225 °C | 392 - 437 °F | |
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Temperature | 190 - 225 °C | 374 - 437 °F | |
Premix Thermoplastics PRE-ELEC® ESD 2300 PRE-ELEC ESD 2300 is a static dissipative thermoplastic compound based on PE-HD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 2300 has been developed for mult.. |
|||
Melt Temperature | 195 - 225 °C | 383 - 437 °F | |
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid.. |
|||
Melt Temperature | 195 - 225 °C | 383 - 437 °F | |
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Melt Temperature | 200 - 225 °C | 392 - 437 °F | |
PTS POM-270 27.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 200 - 225 °C | 392 - 437 °F | |
PTS POM-90 9.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Melt Temperature | 180 - 225 °C | 356 - 437 °F | |
NOVA Chemicals Novapol® LE-0220-A LDPE Extrusion Resin
(discontinued **) Features: easy processing, high melt strength.Applications: wide range of profile extrusions, tape and sheet extrusion, concentrates.Data provided by the manufacturer. |
|||
Melt Temperature | 180 - 225 °C | 356 - 437 °F | |
NOVA Chemicals Novapol® LE-0520-A LDPE Extrusion Resin
(discontinued **) Features: easy processing, good dispersion.Applications: Additive and color concentrates for film and molding.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 225 °C | 383 - 437 °F | |
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Melt Temperature | 185 - 225 °C | 365 - 437 °F | Injection Molding |
LG Chemical KEYFLEX BT 1033D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 185 - 225 °C | 365 - 437 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1033D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 200 - 225 °C | 392 - 437 °F | |
LG Chemical Lucet® N109 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 200 - 225 °C | 392 - 437 °F | |
LG Chemical Lucet® N127 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 180 - 225 °C | 356 - 437 °F | |
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Temperature | 210 - 225 °C | 410 - 437 °F | Molding |
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 205 - 225 °C | 401 - 437 °F | |
Covestro Desmopan® DP 9380A Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin.. |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 220 - 225 °C | 428 - 437 °F | |
Beijing Ranger Chem BLUESTAR® 1079 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Temperature | 220 - 225 °C | 428 - 437 °F | |
Beijing Ranger Chem BLUESTAR® 1084 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Temperature | 220 - 225 °C | 428 - 437 °F | |
Beijing Ranger Chem BLUESTAR® 1110 PBT Can be used directly for spinning, or it can be used after reinforcement & compounding. It can also be used to produce cable sheath through tackificationInformation provided by Beijing Ranger Chemic.. |
|||
Melt Temperature | 220 - 225 °C | 428 - 437 °F | |
Beijing Ranger Chem BLUESTAR® 1135 PBT Can be used directly to produce cable sheathInformation provided by Beijing Ranger Chemical Co. |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 220 - 225 °C | 428 - 437 °F | |
Beijing Ranger Chem BLUESTAR® 1120 PBT Can be used directly to produce cable sheathInformation provided by Beijing Ranger Chemical Co. |
|||
Melt Temperature | 180 - 225 °C | 356 - 437 °F | |
NOVA Chemicals Novapol® LE-0820-AM LDPE Concentrate Resin
(discontinued **) Features: easy processing, good dispersion.Applications: Additive and color concentrates for film and molding, non-critical extrusion coating.Data provided by the manufacturer. |