Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
PolyOne OnFlex™ S EH 40A-3S7001 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
PolyOne OnFlex™ S HS 70A-3E2543 Thermoplastic Elastomer (TPE) This OnFlex™-S HS thermoplastic elastomer compounds is based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver high strength and medium-low density in add.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE Z805P Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYelast TPE Z606 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | |
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Melt Temperature | 185 - 220 °C | 365 - 428 °F | Recommended |
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3028D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding Range |
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Melt Temperature | 160 - 220 °C | 320 - 428 °F | |
Lucobit Lucofin® 1410-t2 Polyolefin TPO Granules, Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t2 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Melt Temperature | 160 - 220 °C | 320 - 428 °F | |
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | |
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | |
Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene EX3 (HM 5010 T2N) is a natural colored high density polyethylene with Butene-1 as comonomer. The product is classified as PE 80 and good stress crack resistance properties combined with good impact .. |
|||
Melt Temperature | 160 - 220 °C | 320 - 428 °F | |
Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BL1481 High Density Polyethylene BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular.. |
|||
Melt Temperature | 182 - 220 °C | 360 - 428 °F | Average value: 204 °C Grade Count:14 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | |
LATI Latimass 52/11-04 D008 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance. This black is formulated to mainta.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection-molding |
BASF Ultraform® W2320 0035 LEV POM Description: Is a POM, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |